Completely in awe of this. Makes me realise how slow and backwards my method of shaping foam is!
I have no experience of fibreglass so terrified of using it, maybe I should just go for it?

Looking forward to your next updates!

Yes you should go for it from the bits I have picked up along the way, dont do it in full sun it will set while your working on it . two thin lairs of CSM is better than one thick one because it wets out easier and holds the shape better. if its very cold add more catalyst.if it goes wrong dont panic let it set cut it out or sand t back and start again.